Joining/welding grade X65 with X60?

118 views
Skip to first unread message

Rouji

unread,
Apr 11, 2020, 3:11:50 AM4/11/20
to Materials & Welding
Greetings,

We have welded X60 crude oil pipeline, and we want to replace a small portion of the pipeline, can we use X65 as replacement?.
Because we have stock of X65.

Thanks.

Ilkin hasanov

unread,
Apr 11, 2020, 3:20:35 AM4/11/20
to material...@googlegroups.com
High grade can cover below grade 
Not vice versa 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eadfb524-1fc1-4f05-adae-de22c88a9b74%40googlegroups.com.

Perumal Govindan

unread,
Apr 11, 2020, 3:46:59 AM4/11/20
to material...@googlegroups.com

Please get design/piping engineering concurrence and get it approval by the client before fitment.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Vinay Thattey

unread,
Apr 12, 2020, 12:20:32 AM4/12/20
to material...@googlegroups.com
The  API 5L pipeline is commonly used for crude oil application.
ASTM-A-106B is very close to that  .  
X indicates minimum yield strength . 
API 5L X65 pipe   is a high level grade pipe in API 5L  with minimum yield strength required in 65000 Ksi or 450 Mpa. 
You can replace but take a view of your designer .


Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

MADHUSOODHANAN NAIR .G

unread,
Apr 12, 2020, 11:46:45 PM4/12/20
to material...@googlegroups.com
Dear All
    Certainly you can weld the  different grade pipes use E6010 for root pass and E7010/E7018-1 for other passes.If the requirement of impact test better to use E7018-1.  
Madhusoodanan Nair.G
 Mob- 7977762694,9967901872