WPS with groove welding will also qualify Fillet welding.

175 views
Skip to first unread message

Mohammed Ghani

unread,
May 21, 2015, 6:03:41 AM5/21/15
to material...@googlegroups.com
Dear Experts, 

Can any one suggest if Groove welding WPS will also allow welding with fillet. please guide with reference standard clause.

--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

gulzar ali

unread,
May 21, 2015, 6:27:19 AM5/21/15
to material...@googlegroups.com
Dear Mohammed Ghani,

please refer ASME SEC-9 para QW-202.2(C) and QW-451.4


Best Regards:
Gulzar Ali
Mob: 00964-7729203068 (IRAQ )
Mob: 0092-333-2833894 (Roaming )

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVjjPwZ%2BkvBBQ-mQ1p1XV0tjtSv4jh8vqu-icwtVMpD%2B7g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

george....@gr.bureauveritas.com

unread,
May 21, 2015, 7:25:01 AM5/21/15
to material...@googlegroups.com

When ASME is the Code, yes
This is not the case for EN 15614-1

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Mohammed Ghani ---21/05/2015 13:13:43---Dear Experts, Can any one suggest if Groove welding WPS will Mohammed Ghani ---21/05/2015 13:13:43---Dear Experts, Can any one suggest if Groove welding WPS will also allow welding with

--

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to


To post to this group, send email to


To view this discussion on the web visit

anosh wankhade

unread,
May 22, 2015, 1:37:11 AM5/22/15
to material...@googlegroups.com

Agreed with Dr. Georgious,

This is listed as non essential Variable in ASME section IX.
Please refer QW : 4.2.30 

Regards,

Anosh Wankhade

For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

JERRY TUAN

unread,
May 23, 2015, 12:22:44 AM5/23/15
to material...@googlegroups.com



Vào 12:37:11 UTC+7 Thứ Sáu, ngày 22 tháng 5 năm 2015, Anosh Wankhade đã viết:

mohd firdaus

unread,
May 23, 2015, 12:23:46 AM5/23/15
to material...@googlegroups.com
What about AWS D1.1?. It is WPS groove cover for fillet?.

Mohd Firdaus Abd Rahim
QA/QC

Sent from my iPhone

On 21 Mei 2015, at 7:24 PTG, george....@gr.bureauveritas.com wrote:

When ASME is the Code, yes
This is not the case for EN 15614-1

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


<graycol.gif>Mohammed Ghani ---21/05/2015 13:13:43---Dear Experts, Can any one suggest if Groove welding WPS will also allow welding with

JERRY TUAN

unread,
May 23, 2015, 12:31:18 AM5/23/15
to material...@googlegroups.com



Vào 12:37:11 UTC+7 Thứ Sáu, ngày 22 tháng 5 năm 2015, Anosh Wankhade đã viết:

meisam shokri arfaei

unread,
May 23, 2015, 12:49:31 AM5/23/15
to material...@googlegroups.com
I Think that the question was about welding and not about qualification.

Whenever a WPS (whether Standard, pre-qualified or qualified) prepared, the manufacturer allow to use it only with values or in the range which mentioned in that WPS.

The qualification has a different story. One or more WPS's may qualified with single PQR (or number of PQR's which are less than the number of WPS's and in some cases one PQR for each WPS) under the criteria and qualification rules of the design and/or qualification code. 

So, in summary, if you have a WPS for welding a groove weld, you allowed to use it just for that. For a fillet weld you should prepare a new WPS. however both may qualified with a single WPS.


Regards




For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer





M.Sathiya Narayanan

unread,
May 26, 2015, 12:49:15 AM5/26/15
to material...@googlegroups.com
Dear

WPS is restricted to what for it is written, some of the WPS written for fillet, Groove,  fillet + Groove 

These are based on Limitation by Qualified PQR 

For your query

what is the reference code for PQR qualification , with that code if the PQR limitations allow to use for both just rewriting the WPS  as per your requirement with PQR limitation will serve you


Regards
M.Sathiyanarayanan





 


For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards
M.Sathyanarayanan

alireza samimi

unread,
May 26, 2015, 1:28:12 AM5/26/15
to material...@googlegroups.com

Kannayeram Gnanapandithan

unread,
May 26, 2015, 1:42:01 AM5/26/15
to materials-welding
as per ASME, without PQR ref , WPS is invalid unless it is SWPS

as code of Sec9, groove weld will qualify Fillet weld also

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY