Thickness Range for Repair welding Procedure.

862 views
Skip to first unread message

Madhu

unread,
Mar 12, 2012, 9:20:35 AM3/12/12
to Materials & Welding
Dear All,

Kindly Share knowledge as details below..


I have Done Repair PQR as per ASME & DEP- SHELL DEP 31 38 01
31, Except Root opening on 12" Superduplex materil X

thickness-17.48mm.Total Deep Excavation is -13.48 mm Except Root
opening (04mm).

As per ASME Sec-IX - QW-202.3 Weld Repair and Buildup. WPS qualified
on groove welds shall be applicable for weld repairs to
groove and fillet welds.
As per DEP31 38 01 31-2.4.2 Welding of duplex stainless steel-The
quality of duplex stainless steel welds very much depends on heat-
input control. The-
3. Repair weld procedures for half wall thickness and cap repairs also
require a PQR.

Now My Query is How much thickness will Qualify In Repair WPS?

Kindly send me some Reference or Details as mention above.


Thanks & Regards

Madhusudan Rout.


Kavin Murugam

unread,
Mar 12, 2012, 9:07:46 PM3/12/12
to material...@googlegroups.com

KINDLY FIND THE ATTCHED SKETCH FOR BETTER UNDERSTANDING.
CORRECT ME IF I'M WRONG.....
 
Kavin Murugam
0126159644

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


1ST PQR.docx

Kavin Murugam

unread,
Mar 12, 2012, 9:13:32 PM3/12/12
to material...@googlegroups.com
RE-SEND WITH EXAMPLE OF WELD RECORD FOR REPAIR PQR
 
Kavin Murugam
0126159644
KNM-PQR-10148 (Fresh) & R1 & R2.pdf

Madhusudan Rout

unread,
Mar 12, 2012, 11:06:12 PM3/12/12
to material...@googlegroups.com, kavin...@yahoo.com

Thanks For Information,

           But As per DEP standard - Only Partial & Cap Repair procedure required , There is no require for root opening.

           Can u send me the any code which will help me regarding Material thickness range Qualifying in WPS  as I mention  previous Discussion.

Thanks..






To unsubscribe from this group, send email to materials-weld...@googlegroups.com

Declan Foley

unread,
Mar 13, 2012, 5:07:41 AM3/13/12
to material...@googlegroups.com

Hi guys,

looking to do a procedure on a pipeline (32" OD x 18mm wt)for bug mig (solid wire) welding using narrow gap technique, anyone got an examples which might be helpful

regards

Declan