Groups
Groups
Sign in
Groups
Groups
Materials & Welding
Conversations
Labels
About
Send feedback
Help
BUS beam
38 views
Skip to first unread message
basem elabd
unread,
Nov 4, 2020, 9:28:20 PM
11/4/20
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
Dear all
@ built-up section beam in welding SAW progress if the web Thk. equal or less than 8mm.
Can welding from one side only or I can't
Thanx
Zacharias Rohith Joseph
unread,
Jan 14, 2021, 5:11:44 AM
1/14/21
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Fillet weld has to be done from both sides.