% Ovality tolerance of A106 seamless pipe

1,184 views
Skip to first unread message

Pattara Karn-Ar-Pakorn

unread,
Jan 21, 2014, 11:54:18 PM1/21/14
to material...@googlegroups.com
I'd like to know the % of ovality tolerance of CS pipe A106 seamless; 8" Sch.STD. Could you please someone can help?
 
Thanks & regards,
 
Pat

Vairamuthu Ramar

unread,
Jan 22, 2014, 10:11:21 AM1/22/14
to material...@googlegroups.com

 hi,
 
pls find the attached file for pipe ovality tolerance.
 
hope it will help you.
 
 

Date: Tue, 21 Jan 2014 20:54:18 -0800
From: pat.fre...@gmail.com
To: material...@googlegroups.com
Subject: [MW:19903] % Ovality tolerance of A106 seamless pipe


I'd like to know the % of ovality tolerance of CS pipe A106 seamless; 8" Sch.STD. Could you please someone can help?
 
Thanks & regards,
 
Pat

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Pipe ovality tolerance - 2 pages.doc

GURDEEPSINGH ARORA

unread,
Jan 23, 2014, 2:09:22 AM1/23/14
to material...@googlegroups.com
Pl. refer ASTM A530 ( General Requirements for Specialized Carbon and Alloy Steel Pipe).

Regards 
G.S.Arora 
Ph: 91-7567125331