REQUIRED FILLER WIRE FOR (ASTM A312-Gr UNS 31254) Super Austenetic Stainless Steel

529 views
Skip to first unread message

Muhammad Azeem

unread,
Feb 7, 2022, 10:18:00 PM2/7/22
to material...@googlegroups.com
Gents,
I need your valuable support to assist about the filler wire to be used for Super Austenitic Stainless Steel (ASTM A 312 Gr UNS 31254) ??




Regards,

Muhammad Azeem Iqbal
Welding Inspector Aramco Approved
053110-8577/0554453626/0590071467


james gerald

unread,
Feb 8, 2022, 12:41:30 AM2/8/22
to material...@googlegroups.com
Please refer attached article.

Thanks & Regards

J.Gerald Jayakumar



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHqH7yAQ5mG4ZSP1b8dm-3X7HWASTFGeuv0Y_s2hqR-qGHH2mw%40mail.gmail.com.
weld-254SMO.pdf

Mohd Siraj

unread,
Feb 8, 2022, 10:18:57 PM2/8/22
to Materials & Welding
Avesta P54 is a good choice for SAS and it is affluently available in KSA, very cost effective.
just take care of good cleaning and avoid any kind of moisture on the surface and hope u pass G48!

P54.pdf

Shahil Saini

unread,
Feb 9, 2022, 2:54:39 AM2/9/22
to material...@googlegroups.com
Hello Everyone,

Why filler wire selection of A 312 UNS 31254 is not mentioned in Table 6 of SA 312 of ASME Sec II Part A1? 
image.png


Muhammad Azeem

unread,
Feb 9, 2022, 2:54:46 AM2/9/22
to material...@googlegroups.com
Dear Siraj,
Thanks for your valuable response, Avesta P54 is a Brand ,I need to check if this manufacturer is approved by Aramco SAP & What is the AWS/SFA number for this filler wire ??

As I consult with 3rd Party they recommend  ERNiCrMo3,F43  ??

Regards,

Muhammad Azeem Iqbal
Welding Inspector Aramco Approved
053110-8577/0554453626/0590071467



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Aqil Abbas

unread,
Feb 9, 2022, 3:05:29 AM2/9/22
to material...@googlegroups.com
Hi,

I believe you should go for ERNiCrMo3/ENiCrMo3. We have used the same filler material for 2-3 of our project with aramco.



--

OPEN TO NEW CONNECTIONS

https://www.linkedin.com/in/aqil-abbas/


Best Regards,

Aqil Abbas

Welding QA/QC Inspector

Saudi Aramco Onshore Maintain Potential Project

Mobile # +966-58-204-4155


james gerald

unread,
Feb 9, 2022, 6:06:57 AM2/9/22
to material...@googlegroups.com
Pls check SA358

Inline image


Thanks & Regards

J.Gerald Jayakumar


Muhammad Azeem

unread,
Feb 9, 2022, 6:06:57 AM2/9/22
to material...@googlegroups.com
Hi Aqil,
As per your given filler wire detail ERNiCrMo3 , I will go with this option .

Regards,

Muhammad Azeem Iqbal
Welding Inspector Aramco Approved
053110-8577/0554453626/0590071467



Muhammad Zulfiqar Ali

unread,
Feb 9, 2022, 6:06:58 AM2/9/22
to material...@googlegroups.com
Dear Azeem,

Please be noted that manufacturing SA approval is not required for these kinds of material, you may procure this material through any approved supplier if needed. 

On Wed, Feb 9, 2022 at 10:54 AM Muhammad Azeem <azee...@gmail.com> wrote:


--

Kind Regards,

M Zulfiqar Ali

Mob: +966 (0) 56 089 1836

Prasad Talari

unread,
Feb 9, 2022, 10:16:26 PM2/9/22
to materials-welding
Hi Iqbal,

ER Ni Cr Mo-3 (F No 43) is the right choice for this , i ve qualified a PQR for this material


Regards
Prasad Talari
Welding Engineer
GAC-Qatar

RIJU PATHROSE

unread,
Feb 9, 2022, 10:16:26 PM2/9/22
to material...@googlegroups.com
FTA

image.png

image.png

On Wed, 9 Feb 2022 at 06:18, Mohd Siraj <mohd...@gmail.com> wrote:
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8e1f3a9f-2d27-44fa-b777-6a9e6ed119ddn%40googlegroups.com.


--
Best Regards,
Riju pathrose
QA/QC Engineer
Mob: +966558506746

Tajuddin Mohammed

unread,
Mar 10, 2022, 10:10:28 PM3/10/22
to material...@googlegroups.com
You can use ERNICRMO-3 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages