Welder qualifications B31.3 K328.2.1(b)

70 views
Skip to first unread message

Vimal Kumar

unread,
May 28, 2020, 11:47:24 PM5/28/20
to material...@googlegroups.com
Dear Experts,

As per the specified clause in subject., does it mean existing qualified welders are to be requalified..??

Kindly advise

Thanks in Advance

Regards
Vimal Kumar
--
Sent from iPhone

TDK YOKESH

unread,
May 30, 2020, 11:20:08 AM5/30/20
to material...@googlegroups.com
Dear Vimal,

What is your design requirement in B31. 3? Chapter v or chapter IX? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO%2BCCQVBBsVK0WYsf9-1mdk91BYE1z6Xxm3MMBwvp2bUM-JwSg%40mail.gmail.com.

Rajnish Dixit

unread,
May 30, 2020, 11:20:10 AM5/30/20
to material...@googlegroups.com
Dear Vimal,
No, it does not say that one has to re-qualify the welders.
It says that :

""b) Test weldments shall be made using the same specification
and type or grade of base metal(s), and the same
specification and classification of filler metal(s) as will be
used in production welding.""

It means if the welders have been qualified as per above conditions, no need to re-qualify the welders.

Hope, your query has been answered.
Thanks,
Best Regards,
Rajnish Dixit
--

TDK YOKESH

unread,
Jun 2, 2020, 11:39:23 AM6/2/20
to material...@googlegroups.com
Dear Vimal,
The K series falls under chapter IX which demands performance qualification by mechanical testing which includes impact testing as well. Also ech product form as used shall be qualified seperstely. Kindly go through chapter IX and interpretations for better understanding. 

Reply all
Reply to author
Forward