Why 2’’ Dia and below size can’t be partially repaired

28 views
Skip to first unread message

Venkadesh Lakshmanan

unread,
Dec 23, 2019, 6:05:06 AM12/23/19
to materials-welding
Gents,

Could you please provide any spec reference regarding 2’’ and below size pipe Welding can’t be partially repaired.

Regards,
Venkadesh 

Hareesh K V

unread,
Dec 23, 2019, 10:08:35 PM12/23/19
to material...@googlegroups.com
Dear Sir, 

Note: Comments based on ASME B31.3 Code

No such restrictions in code as per my knowledge.

We does partial repairs, but the only thing is one should be confident enough to mark the repair based on a DWDI (Ellipse) RT film. 

Regards, 

Hareesh K V

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA_6cSfWXXDgtPxGFo-P9h7dmgu_UXUyaA%3DCyjTejx%3Dna1kz9w%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages