We have a welded joint: stainless steel type 6Mo UNS S31254 using filler metal ERNiCrMo-3. What would be the chemical requirements criteria ( Cr, Ni, Mo)  be for PMI on this joint? Any standard/ code for reference? 

--




Perumal Govindan

no leída,
9 dic 2021, 1:25:499/12/21
a material...@googlegroups.com,Pham Thuc
While welding dissimilar materials, usually lower grade properties shall be acceptable and its a normal industrial practice.

For more information, pease refer your welding specifications of.your project.

Regards 
P Govindan 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADOyxJi%2BOSmeuJhmc8e-hvB8c8hMHnzXBMAkX8WuJ9tzJhdrnw%40mail.gmail.com.

anhtrangnghieng

no leída,
9 dic 2021, 3:52:169/12/21
a material...@googlegroups.com,Pham Thuc
Dear Mr. Govindan, 

Do you mean in this case, acceptance criteria shall be in red color as below ? 

6Mo weld to 6Mo
Cr Ni Mo
A312 S31254 (6Mo) 19.5-20.5 17.5-18.5 6-6.5
A312 S31254 (6Mo) 19.5-20.5 17.5-18.5 6-6.5
ERNiCrMo-3 20-23 58 min 8-10
Weld metal required 19.5 17.5 6