Multiple welders on single production joint

306 views
Skip to first unread message

Prasu Cutie

unread,
Aug 9, 2016, 10:11:14 PM8/9/16
to material...@googlegroups.com

Dear experts,

I have a query n looking  for earliest  response
I had welders qualified on 1/2" OD with 7.46mm thk
Now we had a production joint of 2" OD with 8.75mm thk, which is required  to be    done with full tig

Now the question is, Can we engage two 1/2" qualified welders to weld 8.75mm thk??
Is there any clause in sec.ix for having two welders on single production joint to cater excess thk??
Or should we go for separate qualification using 2 welders on single test cupon??
Plz update me the clause no. If it is allowed

Awaitng for your quick response

Thank you all

Regards
Prasad

venkat chikkala

unread,
Aug 10, 2016, 2:17:25 AM8/10/16
to material...@googlegroups.com
Dear Prasad,

As per ASME Sec IX, Two welders can be used in single production joint full filling all other essential veriables as welder is qualified based on weld metal thickness not on base metal thickness.

Each welder can deposit maximum 7.46 mm only, which he qualified

You must have supporting WPS to weld 8.75 mm thk  with TIG.

Refer QW 306 and QW 351. 

You check client specification for any specific requirements

Regards,
CH V Ramana
BVIL


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKgcArTBn1q8qXcabJnNuhU2zCFy3p6H5LJMOsvZJv6jS07cXg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


dili...@gmail.com

unread,
Aug 11, 2016, 2:31:03 AM8/11/16
to Prasu Cutie
Your description is not very accurate but I think that you can proceed

Sent from my BlackBerry 10 smartphone.
From: Prasu Cutie
Sent: Τετάρτη, 10 Αυγούστου 2016 - 05:11
Subject: [MW:25236] Multiple welders on single production joint

--
Reply all
Reply to author
Forward
0 new messages