Respected Experts,

Had a discussion at a customer site on subject.

Is Weld Map a must for each - WPS PQR, like a vessel fabrication drawing has?

Please share, some knowledge. We need to weld process pipes ranging from 2" to 16" (seamless sch. 40 to sch 160) and hence the request.

Best regards,

Vinod Bhatt
Vinod Bhatt

Raghuram Bathula

unread,
Feb 12, 2013, 11:30:43 PM2/12/13
to material...@googlegroups.com
Weld map is part your QC documentation to correlate each weld or a group of similar welds to the applicable WPS. it can be either a line sketch, tabular or in any other form. 

You can prepare an index of all the WPS applicable for this project and indiacte WPS number against the each piping class. it is the easiest way.

Binoy Soman

unread,
Feb 12, 2013, 11:30:18 PM2/12/13
to material...@googlegroups.com
It is not necessary.
Usually we include the joint type details along with WPS.
sumod
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


Vimal Mistry

unread,
Feb 13, 2013, 5:30:32 AM2/13/13
to material...@googlegroups.com
Dear Mr. Vinod.

It's not necessary but customer could be asked for this as its giving at a glance idea for your qualified WPS range which is acceptable for his job or not? So if you had submitted your WPS then customer can verify or Approve the same.

You can refer attached table

Best Regards,

Vimal Mistry
SEL-QA

-----Original Message-----
From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Vinod Bhatt
Sent: 12 February 2013 22:33
To: material...@googlegroups.com
Subject: [MW:16752] Weld Map - WPS PQR

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



------Disclaimer-------
This email and any files transmitted with it are confidential and may be privileged or otherwise protected from disclosure and are intended solely for the use of the entity / individual to whom they are addressed. If you have received this email in error or If you are not the intended recipient, please notify the sender immediately by way of telephone or email and delete this message and any files transmitted from your system. Please note that any views presented in the email are solely those of the author and do not necessarily represent those of the organization. While all care has been taken to avoid viruses the recipient is advised to check this email and attachments for presence of viruses. The organization accepts no liability on this account.
------Disclaimer-------
Untitled.png

kannayeram gnanapandithan

unread,
Feb 13, 2013, 5:51:30 AM2/13/13
to material...@googlegroups.com
What Raghuram said is the Best & Easy method to understand by Taskperformars.
Pl do carry out Weldmap/Weld matrix/Weldplan whatever way u want
Pandithan
Welding Consultant

SmartWeld

unread,
Jul 12, 2015, 11:22:44 PM7/12/15
to material...@googlegroups.com, vnb...@gmail.com
Hi all

Weld mapping is the process of assigning information to a weld joint to enable easy identification of its design (WPS), production (welders, their qualifications, date welded), quality (visual inspection, NDT) and traceability (heat numbers of materials joined & welding consumables). 

Weld mapping should also incorporate a pictorial identification to represent the weld number on the fabrication drawing, in case the designer does not nominate a weld number. 

To manage this multi-stage labour intensive record keeping activity, cloud-based welding management software such as Smart Welding Manager, with its Android and iOS tablet apps will reduce the workload and minimize the errors as it distributes the work across the production hierarchy.

Regards

Shaik Basha

unread,
Jul 15, 2015, 1:58:30 AM7/15/15
to material...@googlegroups.com
Not required. Joint details can be shown in isometric drawing with joint details

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Saravanan Sornam

unread,
Jul 16, 2015, 2:28:34 AM7/16/15
to material...@googlegroups.com
Dear Vinod,

let me ask you a Question.

Incase, the WPS No. & the Joint No. is not prescribed in fabrication Dwg, 
and if you have 20 no. of weld joints in a Vessel, which is to be welded with 3 different WPSs,
for example GTAW only for below 3" Nozzles , GTAW + FCAW combination welding , GTAW + FCAW + SAW combination for Long Seams ,

you have to give each Joint No. , the applicable WPS No. for that Joint and NDT method for those joints, that is the reason that the customer is asking for a Weldmap .

If customer requests you to issue Weld Map , then you have to submit it and to make them understand with full details of Welding .

Simply submitting only the WPSs for all of the 20 No. of weld joints would make confusions and mess, even to your own fabrication team also.

Regards,
Saravanan,
Korea

Oscar Soldadura

unread,
Apr 17, 2017, 11:45:27 PM4/17/17
to Materials & Welding, vnb...@gmail.com
buenos dias, 

Hay alguna norma que me indique cuales son los items minimos para registrar en un Weld Map

Gracias

Good morning

Is there a rule (code or standard) that tells me what the minimum articles are for registering on a Weld Map.

Thanks

My client is asking me for the following:

Heat input, preheat and interpass