PQR for carbon steel with S'S lined

88 views
Skip to first unread message

Irfan Mohammed

unread,
Feb 13, 2015, 10:53:25 AM2/13/15
to material...@googlegroups.com

Dear experts,
I have a situation I have to weld CS with SS lined pipe to CS with SS lined elbow.
CS pipe 10"/21.9mm with S'S clad 3mm internally
Pwht required, impact test not required.
Code of qualification- SEC IX & ASME Div II requirements.
Request you all to please advise on possible PQR qualification scenarios.

Thanks
Irfan

Rems Okonkwo

unread,
Feb 13, 2015, 11:09:54 PM2/13/15
to material...@googlegroups.com

Dear Irfan,

You will have to provide more details like the St detail,  the CS details and the operating characteristics (MDMT)

Regards,

Rems
IWE Nigeria

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXGqGQxi3-Q2OW_Sa5OhZ4oraEDBYnd-MVtR1Z4JFix12AHKA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Raghuram Bathula

unread,
Feb 13, 2015, 11:19:21 PM2/13/15
to Materials-Welding
Dear Irfan

Read QW217  requirements,  either (a) or (b) whichever is applicable to your case, then put forward your proposal, in case if you need further clarifications.........

Irfan Mohammed

unread,
Feb 14, 2015, 12:25:17 PM2/14/15
to material...@googlegroups.com

Dear raghuram,
Thnx fir the info I have checked in  QW 217 requirements and my case falls in QW 217 (b) becomes our cladding part is not included in design

Thnx to all for ur support
Irfan.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.