Dear all,

Our contract document is restricted for FCAW process upto 25 mm thickness and design temperature not less than minus 10 degree centrigrad for all pipe welding.

Any specific reason for the  limitation of particular process.

Thanks in advance.
Pradip

pgoswami

unread,
Oct 25, 2022, 12:04:01 AM10/25/22
to pradip kumar Sil, materials-welding, pgos...@rogers.com
Pradip, 
The spec seems to be outdated. There're scopes for improvement. You may refer latest API RP 582 for guidance, as well as the other industry standards & consumable manufacturer's guidebooks. 
Hope this will help. 

Thanks. 
P.Goswami, P.Eng,IWE



Sent from my Bell Samsung device over Canada's largest network.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DKz1LWV0ofaEnFpSnWDXoaAo_utePdx_MKfbg%2B7CzmEQ%40mail.gmail.com.

Kannayeram Gnanapandithan

unread,
Oct 25, 2022, 11:29:13 PM10/25/22
to materials-welding
if it is solid wire, ur spec ok because  different metal transfer. For FCAW  to my knowledge,  no restrictions 

--