GB Standard equivalency

248 views
Skip to first unread message

Endri Prasetyo

unread,
Feb 11, 2011, 3:15:20 AM2/11/11
to material...@googlegroups.com
Dear Member,

Anybody can inform what is the GB standard number which is equivalent to ASME VIII and IX?

Much appreciated for your sharing information on this.

Regards,
Endri

Bathula Raghuram (Mumbai - PIPING)

unread,
Feb 11, 2011, 3:26:27 AM2/11/11
to material...@googlegroups.com

Steel Pressure Vessels GB150

Steel Tubular Heat Exchangers GB151

Roy LIU刘艺

unread,
Feb 11, 2011, 4:12:01 AM2/11/11
to material...@googlegroups.com
Hi, all
GB is China National Standard,  Chinese Pinyin "Guo Biao", we say GB in short.
 
you are right that GB is equivalent to ASME code, but it is hard to distinguish every standard now.
you may search on internet and find helpful information.


 

Best regards

 

Roy LIU

 

Böhler Welding Group - China



Date: Fri, 11 Feb 2011 15:15:20 +0700

Subject: [MW:9818] GB Standard equivalency
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Yassein Abdou

unread,
Feb 12, 2011, 8:45:04 AM2/12/11
to material...@googlegroups.com

Dear All,

                Attached a comparison sheet between different standards, including GB standard

 

Best regards, 

Yassein Abdou

Welding & Grating Manager

energya STEEL FABRICATION 

 

 

 

 

 

 


Egypt Factory & Head Office: Industrial Zone A 6 East, 10th of Ramadan City

Tel         +2015 412 239 - 412 249 / +2010 002 0133

Fax        +2015 412 236

Cairo Office: 98 a Hassan Mamoun St. Naser City, Cairo Egypt

Tel         +2 02 22706306 - 2714 631 Fax +2 02 22752 701

KSA Factory: Rabigh - Yanbu High Way Exit 927 Industrial Zone Aramco Road

Tel:          +966 500 150 706 Fax : +966 500 592

Jeddah Office: Haifa Building. King Road  Jeddah City, Saudi Arabia

Tel         +966 2 2907382  Fax +966 2 6882901

www.energyasteel.com           in...@energyasteel.com

Personal Mobile: + 2010 0400361     email: yassei...@energyasteel.com

 

 


image001.jpg
image002.jpg
Comparison table.pdf