I need to qualify a PQR for SA 335 Gr P9 pipe welding. We have plate SA 387 Gr 9.
But I don't find P number allocated for SA387 Gr 9, and UNS number is matching. Can we consider the P number as 5B?
Someone may object that it is unlisted material??
Please advise and share your thoughts on this why this particular plate grade is not listed in p number table.
.
With regards, 
SATHEESH KUMAR.P 

Karthik

unread,
Jan 15, 2020, 12:00:04 AM1/15/20
to material...@googlegroups.com
Hi,
Its P.No.5B. Please find below extraction from Section IX

Inline image



Thanks& Regards,

 

(Karthik)

Karthikeyan.S

E-mail : karthi...@yahoo.com



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOX%2BP-vWLeYMzcVvFGukWKcpXU4BFF0c-rNidsBiFNNBLdU3SQ%40mail.gmail.com.

José Juan Jiménez Alejandro

unread,
Jan 15, 2020, 12:00:04 AM1/15/20
to material...@googlegroups.com
Please review Table QB / QW-422,   ASME Section IX.
Greetings!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOX%2BP-vWLeYMzcVvFGukWKcpXU4BFF0c-rNidsBiFNNBLdU3SQ%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





Reply all
Reply to author
Forward
0 new messages