P1 Gr1 PQR with impact will support P1/S1 Gr2 material?

490 views
Skip to first unread message

Chandra, Vasanthan (Lagos)

unread,
Jan 7, 2010, 11:33:41 AM1/7/10
to Chandra, Vasanthan (Lagos), material...@googlegroups.com

Friends,

 

I have come across a typical issue as below,

 

  1. Material is API 5L X-65 – S No 1 Gr.2
  2. Impact required at -29 deg.C
  3. Welding as per ASME Sec IX

 

I have a PQR which is SA 106 Gr B (P1 Gr 1) Impact tested at -30 deg.C

 

Can I support this PQR for S1 Gr 2 or P1 Gr 2? My client is rejected this and asking for PQR which was done on Group 2 materials either on S1 or P1.

 

Could you let me know, since my client is seeking evidence as per Sec IX? How to convince them that Gr 1 impact tested can also be used for Gr 2 materials.

 

 

 

Regards,

Vasanth

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

Raghuram Bathula

unread,
Jan 7, 2010, 11:50:41 AM1/7/10
to Materials & Welding
Group Number is a supplementary essential variable, hence new PQR
required, also check if your construction code is B31.3 then you must
qualify the PQR on X65 material only.


On Jan 7, 9:33 pm, "Chandra, Vasanthan (Lagos)"


<Vasanthan.Chan...@DeltaAfrik.com> wrote:
> Friends,
>
> I have come across a typical issue as below,
>

> 1.      Material is API 5L X-65 - S No 1 Gr.2
> 2.      Impact required at -29 deg.C
> 3.      Welding as per ASME Sec IX

G.Alagarasan

unread,
Jan 7, 2010, 10:30:47 PM1/7/10
to Vasantha...@deltaafrik.com, material...@googlegroups.com
Vasanth,

Please review the PQR MTC.. is there any chance that ur mill certs have dual classification...I am sure some of the reputed mfr classify the material as per API and ASME too..

If yes, there is no need for new qualification & but you need to revise the PQR.

Orelse, qualify a new procedure along PTC for Gr2 HAZ impact test..

Alagu

On Thu, 07 Jan 2010 22:19:25 +0530 wrote

>



Friends,



I have come across a typical issue as below,




Material is API 5L X-65 –
S No 1 Gr.2

Impact required at -29 deg.C
Welding as per ASME Sec IX




I have a PQR which is SA 106 Gr B (P1 Gr 1) Impact tested at
-30 deg.C



Can I support this PQR for S1 Gr 2 or P1 Gr 2? My client is
rejected this and asking for PQR which was done on Group 2 materials either on
S1 or P1.



Could you let me know, since my client is seeking evidence
as per Sec IX? How to convince them that Gr 1 impact tested can also be used
for Gr 2 materials.







Regards,

Vasanth





*** WORLEYPARSONS GROUP NOTICE ***
"This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it.
If you have received this email in error, please notify us immediately by return email and delete the email and any attachments.
Any personal views or opinions expressed by the writer may not
necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."





--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

vipin george

unread,
Jan 8, 2010, 9:32:43 AM1/8/10
to material...@googlegroups.com
Hi!
Impact testing is a supllementary essential variable, Hence you need to run a pqr for P.No.1 Gr.2 material.
 
Regards,
vipin george

Reply all
Reply to author
Forward