Regarding PMI for UNS 31254 materials weld

36 views
Skip to first unread message

Dinesh Ravi Shankar

unread,
Feb 1, 2012, 2:29:50 AM2/1/12
to material...@googlegroups.com
 
 Dear Experts,
 
Hope you are doing well.
 
Please find attached PMI report of Super Austenitic Stainless Steel (UNS 31254) welding which used Er NiCrMo-3 filler wire.
 
Then inspection review of Positive Material Identification (PMI) of UNS 31254 materials through NITON Machine, i verified on weld metal using filler Er NiCrMo-3/UNS N06625 that showing UNS N07725 grade and its element contents also as per ASME Sec II, Part C.
 
Please advise.
 
We are QC persons has follow as per Codes & Standards for acceptance, but some case our supervisor/Team lead says overtake the Codes & Standards .What we have to do  & where we have to complaint ?
 
 
 
Thank you & Best Regards,

S. Dinesh Ravi Shankar.
Mechanical Inspector,
Saudi Aramco Project Inspection Division (SAPID),
Manifa Core Hydrocarbon Facilities Project.
Kingdom of Saudi Arabia.,
Mobile : +966 562944695,
Tel      : +966 3 379 2018.
 
 