Dear All,
Can anybody tell me,
what's the ovality tolerance of cylindrical shell pressure vessel (ID 4300 mm and plate thickness 12mm).
Regards,
Anil
|
Dear Anil
Please refer UG80 of Sec VIII Div 1 You can have 1% ovality is acceptable but It is case to case basis i.e Higher the Dia , it should be kept less than 0.5% even the acceptable tolerance is high b) higher ovality will cause more offset in weld seam
ii) In case of heat exchanger , You can not afford to accept higher ovality . You should target less than 0.25% ,Higher ovality will give problem in tube bundle insertion.
Regards
Hegde P.B.
From:
material...@googlegroups.com [mailto:material...@googlegroups.com] On
Behalf Of N Anilkumar
Sent: Wednesday, May 13, 2009 4:04 PM
To: material...@googlegroups.com
Subject: [MW:2184] Ovality tolerance
|
Dear All, |
For this Inner dimension (4300mm), if we target %0,25. Is that mean about +-102mm ?
Regards,
__________ Information from ESET NOD32 Antivirus, version of virus signature database
4070 (20090513) __________
The message was checked by ESET NOD32 Antivirus.
http://www.eset.com
__________ Information from ESET NOD32 Antivirus, version of virus signature
database 4081 (20090517) __________
The message was checked by ESET NOD32 Antivirus.
http://www.eset.com