L-SEAM WELD JOINT DISTANCE

97 views
Skip to first unread message

krishna magdum

unread,
May 17, 2022, 11:16:39 PM5/17/22
to Materials & Welding
Dear team,

pls suggest how much distance required for two L seam joint in pipe, some of people suggest for 4T 

pls suggest for ASME Standard or code

Regards 
Krishna

SENTHILKUMAR SWAMINATHAN

unread,
May 18, 2022, 1:01:54 AM5/18/22
to material...@googlegroups.com
As per ASME Sec. VIII D1, UW8 - (d)
Except when the longitudinal joints are radiographed 4 in. (100 mm) each side of each circumferential welded intersection, vessels made up of two or more courses shall have the centers of the welded longitudinal joints of adjacent courses staggered or separated by a distance of at least five times the thickness of the thicker plate.

Thank you, 
Regards, 
S.SENTHILKUMAR


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2bd671f0-a3c8-4cfc-93d6-d7e9599873e0n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages