Is pressure drop(very small) acceptable in piping during hydro test beyond temperature variations. Please advice.

Regards

Nishanth

Mohd Siraj

unread,
Jan 1, 2016, 1:20:47 PM1/1/16
to Materials & Welding
what is code
test mediam
presaure test?

Mohd Siraj

unread,
Jan 1, 2016, 7:05:15 PM1/1/16
to Materials & Welding
what is code 31.4 or 31.3?
test mediam
test pressure
length of pipeline
line geomentry..

Lakshman

unread,
Jan 2, 2016, 12:06:26 AM1/2/16
to material...@googlegroups.com

Hi friend,

Please elaborate the query with necessary details to look in to that.

 

Thanks & Regards,

Lakshman Kumar B,

9440031459.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Ba8N2%2Bez91HCXKpWy%2B-RFqCAgpKOsKs6OjSOOggmxWtcY43Kw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Nachhattar Singh

unread,
Jan 2, 2016, 3:29:48 AM1/2/16
to material...@googlegroups.com

Dear Friends

 

Per your say a very small drop in pressure - 

Note that a very small is no where acceptable, but there are exceptions that may say “ so many drops per minte” etc.

So you need to be very specific

 

N. Singh

 

Maharashtra, India.

 