Re: [MW:21518] Reinforcing Pad Tale Hole/Testing Port Shall be seal welded after pressure test.

466 views
Skip to first unread message

Shridev Kurup

unread,
Aug 3, 2014, 9:35:51 PM8/3/14
to material...@googlegroups.com

Dear

Please refer Asme sec viii div 1 2013 clause UG 25 (e) & UG 37 d (g)

These telltale holes shall be left open or plugged if vessel I  service. If plugged , the plugging material used shall not be capable of sustaining pressure betwee plate and vessel wall

Regards
Shridev
On 3 Aug 2014 19:42, "sudhakar kuppuswamy" <mechsu...@gmail.com> wrote:
>
> Hi,
>
> Not required to weld tale hole after pressure testing
>
> Chance for residual gases presence are high, if you seal weld it , during operation due to high temperatures gases may expand and lead to failure if it is thin wall.(in rare cases it occurs, so not adviceable to do seal welding)
>
> Regards
> Sudhakar.K
>
> On Jul 20, 2014 2:58 PM, "Yemmina Madhusudhan" <yemminama...@gmail.com> wrote:
>>
>> Is there any standard which states weep hole to be seal welded after completion pressure test.
>>
>>
>> Regards
>>
>> Yemmina Madhusudhan
>> Mechanical Engineer
>>
>> --
>> To post to this group, send email to material...@googlegroups.com
>> To unsubscribe from this group, send email to materials-weld...@googlegroups.com
>> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>>  
>> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
>> For more options, visit https://groups.google.com/d/optout.
>
> --
> To post to this group, send email to material...@googlegroups.com
> To unsubscribe from this group, send email to materials-weld...@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>  
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.

Raja Meurdu

unread,
Aug 4, 2014, 5:26:51 AM8/4/14
to material...@googlegroups.com
Dear Sir,

You could pluged it using kind rubber. Better not to sealed it permanently. When you want to perform corrotion test, you need an acces to tale-tale hole.‎ 

Regards
Teuku Machfud
Dari: Shridev Kurup
Terkirim: Senin, 4 Agustus 2014 08.35
Perihal: Re: [MW:21522] Reinforcing Pad Tale Hole/Testing Port Shall be seal welded after pressure test.
Reply all
Reply to author
Forward
0 new messages