Query related to WPS

245 views
Skip to first unread message

Manish Kumar

unread,
Oct 21, 2020, 10:12:59 AM10/21/20
to material...@googlegroups.com
Dear Sir,
If P number of material 1 & group number 1 & 2 is mentioned in WPS.While supporting relevant PQR is P number 1 & group number only 2. In this case,Will WPS be valid for relevant PQR.

Please advise us .

Attachment-
WPS & PQR 

--
Regards

Manish Kumar
Inspection(Mechanical) Engineer
PDIL-HURL Barauni site
WPS & PQR...pdf

Nithin Joseph

unread,
Oct 21, 2020, 10:36:44 AM10/21/20
to material...@googlegroups.com
Yes, it is correct, for non impact applications. When impact requirement applies, group number becomes essential.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k78r-LmTKgXVDyMf_9wE9PtMAo_C8QBbsd6aqpTaHWgwg%40mail.gmail.com.

Hany Nabil

unread,
Oct 21, 2020, 10:36:52 AM10/21/20
to material...@googlegroups.com
Dear Sir,

For your question 

Yes, a WPS is valid based on mentioned PQR as per ASME- IX code.

Because only P number essential variable and group number is not essential variable.


Thanks & Regards
Hany Nabil 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k78r-LmTKgXVDyMf_9wE9PtMAo_C8QBbsd6aqpTaHWgwg%40mail.gmail.com.
--


 Best Regards,

 Eng. Hany Nabil
 Senior Welding Engineer
 Petrofac
 Engineering and Production Service
 Egypt Mobile: 002-01225622022




This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

Manish Kumar

unread,
Oct 21, 2020, 11:12:37 AM10/21/20
to material...@googlegroups.com
Dear Sir,
With ref.. to the trailing email,P number is essential & Group number is supplementary variable,When impact value is required group number becomes essential. As per attachment of WPS & PQR  impact value is required at Heat affected zone.In this case,how will attached  PQR (P  number 1 & group number 2) be valid for P number 01 Group number 1 & 2.Pl advise me on this concern.
image.png

WPS & PQR...pdf

atul khatri

unread,
Oct 22, 2020, 8:14:15 AM10/22/20
to material...@googlegroups.com
Dear Mr. Manish,

As in this case , you have the impact test requirement, then two separate PQRs shall be required for..

P.No 1, Gr.No 1 to P.No 1, G.No 1
P.No 1, Gr.No 2 to P.no 1, G.No 2

QW-403.5 states..
 
If materials differ only by group number (SAME P-number) and all other essential and supplementary essential variables are the same for two PQR’s joining one group number to itself and the second group number to itself, then the dissimilar group number combination is considered to be qualified. So you can use these PQRs to qualify WPS for P.No 1 Gr.No 1 to P.No 1 to G.No 2.

Hope it clarifies 

Regards,
Atul Khatri
Principal Engineer- Piping
Haldor Topsoe India Pvt. Ltd


udaya bhaskar

unread,
Oct 22, 2020, 10:55:57 AM10/22/20
to material...@googlegroups.com
Dear manish,

Material in whichever mention in PQR is  A/SA–516 70 K02700 70 (485) 1 2 101 100 11.1 C–Mn–Si Plate this is under P1G1.
maybe it was a typing error in WPS, in this case Group number is not countable.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k78r-LmTKgXVDyMf_9wE9PtMAo_C8QBbsd6aqpTaHWgwg%40mail.gmail.com.


--
With Regards

Udaya bahaskar.D

George Dilintas

unread,
Oct 30, 2020, 9:06:36 PM10/30/20
to material...@googlegroups.com
If construction code does not require impact testing then yes

--

Bien_ND

unread,
Nov 1, 2020, 5:36:35 AM11/1/20
to Materials & Welding
Yes, if your PQR qualified on single test coupon, see QW-202.4 b) -2).