material identification as per PMI results

34 views
Skip to first unread message

Elshan Feyzullayev

unread,
Jan 22, 2016, 10:16:09 PM1/22/16
to material...@googlegroups.com

Gents


There is a PMI test result which is as follows:


Ni-0.18%, Cr-1.37%, Fe-96.50%, Mn-0.84%, Mo-0.22%. This is a piece of steel pin. Can anyone suggest the rough material grade that this pin has been made off?


Your thoughts will be highly appreciated.


Many thanks

C.Muni

unread,
Jan 22, 2016, 10:25:59 PM1/22/16
to material...@googlegroups.com
Its 1 Cr 0.5 Mo low alloy steel

Regards,


 Muniyandi Chithiran MBA.,MIIF,
AWS Certified Welding Inspector,
ISO 9001,14001,17025, Lead Auditor,
NDT Level II-RT,UT,MT,PT,

Mobile: 0091 95855 40965,99947 65591

Go where you are celebrated not where you are tolerated.
Comfort is the enemy of achievement.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/HE1PR05MB14334D0F0276A78D94D9CF87EBC40%40HE1PR05MB1433.eurprd05.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.

Lu, Feng

unread,
Jan 25, 2016, 8:09:22 AM1/25/16
to material...@googlegroups.com

It seems to be 4130 but you may further check carbon content to see if it is close to 0.3%.

--