Difference between AWS D1.1 & ASME Sec IX

59 views
Skip to first unread message

Hrushikesh Sangamnerkar

unread,
Jan 9, 2021, 2:58:59 AM1/9/21
to Materials & Welding
Dear all,
Kindly share the Difference between AWS D1.1 & ASME Sec IX, if available.

Thank you

Vishwas Keskar

unread,
Jan 10, 2021, 10:16:24 PM1/10/21
to material...@googlegroups.com
AWS D1.1. - This is for  welding qualification in structural  welding application
                     There are pre qualified WPS s. 
                     Refer respective  chapters for qualification.

ASME SEC IX - This is for welding qualification for pressure  pressure part to pressure part   and pressure  pressure part to non pressure part welding application.
PQR needs to qualify WPS 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2rz_WF%2BEKTwA2AAvFfartFgVncf%2BZ3ceGRsgejGRpJ9bw%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages