I am not able to find mechanical properties/other details/equivalent of AISI 86 30H.I was wondering if  any of the member could throw some light in this regard. All I know is it is to be used as an end fitting for a riser.

Thanks 

saravanan eaganathan

unread,
Jul 24, 2011, 1:35:23 AM7/24/11
to material...@googlegroups.com, vikas.bh...@gmail.com
Dear all,
 
            Please see the below details
 
 
AISI 8630H
Category  Steel
Class  Alloy steel
Type  H-steel
Common Names  Nickel-chromium-molybdenum steel
Designations  Germany: DIN 1.6545
Italy: UNI 30 NiCrMo 2 KB
United States: ASTM A304 , SAE J1268 , UNS H86300

Composition
Element Weight %
C  0.27-0.33 
Mn  0.60-0.95 
Cr  0.35-0.65 
Ni  0.35-0.75 
Mo  0.15-0.25 
P  0.035 
S  0.040 
Si  0.15-0.30 

Mechanical Properties
Properties  Conditions 
T (°C) Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 565  25  annealed at 845°C  more
Yield Strength (Mpa) 370 
Elongation (%) 29 
Reduction in Area (%) 59 
Hardness (HB) 156  25  annealed at 845°C more

Thermal Properties

Properties  Conditions 
T (°C) Treatment
Thermal Expansion (10-6/ºC) 11.2  21-100 more  


Regards
 
saravanan

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Reply all
Reply to author
Forward
0 new messages