Hard Facing_Stellite 6 _reg

51 views
Skip to first unread message

Sivaraman N

unread,
Aug 28, 2016, 11:51:44 PM8/28/16
to Materials & Welding
Dear all,

While doing Hard facing Overlay of stellite 6  on carbon steel and stainless steel  cracks observed during second layer and third layer


Base Material:SA 516 Gr 70 (15 mm thk) & SA 240 TP 316 L(15 mm thk)
Electrode:ECoCrA
Process: SMAW
Overlay thickness:6 mm

How to avoid the cracks during hard facing?

defrih...@gmail.com

unread,
Aug 29, 2016, 2:54:51 AM8/29/16
to Materials & Welding
Mr Siva

How about your travel speed during welding.?


Defri


QA/QC Inspector
+6281286886600

Shyamal Das

unread,
Aug 29, 2016, 3:23:53 AM8/29/16
to material...@googlegroups.com
HI

Did you use any Buffer layer prior to ST6, if not use E312 XX type electrodes as a base layer .

use stringer bead

regards

DAS

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8afcb0ec-7cc7-4414-be0c-f3a4d82b5f32%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Gopalakrishnan G

unread,
May 30, 2019, 9:15:27 AM5/30/19
to material...@googlegroups.com
Me to facing the same problem....kindly guide me. 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages