Bevel end preparation for butt weld

368 views
Skip to first unread message

harsha bhat

unread,
Feb 15, 2012, 10:24:12 AM2/15/12
to material...@googlegroups.com
Dear Experts,

I have a doubt pertaining to the bevel ends preparation as per ASME B16.25.

While defining the type of end preparation for butt welding as per ASME B16.25, say for e.g. for nominal wall thickness greater than 25 mm GTAW root pass, on what basis do we decide the type of the bevelled ends in Fig.6. i.e. is it type A or Type B?

Apart from the wall thickness what are the other parameters to be considered to select type of bevel ends from Fig.2(a), Fig,3(b)...etc. from ASME B 16.25. Is the base material also a parameter which governs for the selection of the type of bevel end preparation for butt welding?

I request if any of you could guide me. Thanking you all in advance,

Regards,
Harsha Bhat.

narasimha murthy

unread,
Feb 24, 2012, 4:57:57 AM2/24/12
to material...@googlegroups.com
Dear Harsha,

In ASME B 16.25 , The SECTION 1.Scope PARA 1.1 General and  1.2 Application clearly states where and how this standard is applicable,
hope you could read through and clarify.

Regards,

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.