B31.3 Piping Ovality limits

2,327 views
Skip to first unread message

Lassaad

unread,
Apr 27, 2014, 1:51:49 PM4/27/14
to material...@googlegroups.com
Dear Experts,
What are the ovality limits for piping as per B31.3?
Many thanks

Sent from my ThinkPad S230u

AHMAD&MOHAMAD REDA

unread,
Apr 29, 2014, 4:24:53 AM4/29/14
to material...@googlegroups.com
Dear mok
there is no straight mention to ovality as per B31.3 and the only presence to diameter tolerance is the next snapshot (332.2 bending)
and i think it can works


 

OUR BEST REGARDS

AHMAD AND MOHAMAD REDA

01223964394 & 01223932379

SENIOR QA-QC

PETROJET 

Lassaad Mokrani

unread,
Apr 29, 2014, 9:22:15 AM4/29/14
to material...@googlegroups.com
Many Thanks Amer,
Could you resend the snap shot on an other format.
I can't get it
Thanks

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Meilleures salutations

MOKRANI Lassaad
Consultant Civil Engineer
Tunisia
00216 20 649 755
http://www.linkedin.com/pub/lassaad-mokrani/16/364/907


















P     Pensez environnement! N'imprimez ce mail que si c'est vraiment nécessaire
Please consider your environmental responsibility before printing this e-mail


This e-mail is confidential and it is intended only for the addressees. Any
review, dissemination, distribution, or copying of this message by persons
or entities other than the intended recipient is prohibited. If you have
received this e-mail in error, kindly notify us immediately by telephone or
e-mail and delete the message from your system. The sender does not accept
liability for any errors or omissions in the contents of this message which
may arise as a result of the e-mail transmission

Vairamuthu Ramar

unread,
Apr 29, 2014, 11:11:33 PM4/29/14
to material...@googlegroups.com
Dear Sir,
 
The attached file might be useful regarding ovality tolerance.
 

 

Date: Tue, 29 Apr 2014 15:22:15 +0200
Subject: Re: [MW:20699] Re: B31.3 Piping Ovality limits
From: lassaad...@gmail.com
To: material...@googlegroups.com
Pipe ovality tolerance - 2 pages.doc

AHMAD&MOHAMAD REDA

unread,
May 1, 2014, 7:54:54 AM5/1/14
to material...@googlegroups.com
attached and i hope u get it


OUR BEST REGARDS

AHMAD AND MOHAMAD REDA

01223964394 & 01223932379

SENIOR QA-QC

PETROJET



332.2.doc

joseph mbé

unread,
May 3, 2014, 5:39:12 AM5/3/14
to material...@googlegroups.com
Hi,

Go to pipe fabrication codes or standards such as APL 5L line pipe specification

regards
 
Joseph Faustin Mbe
QA/QC Engineer
TEL CMR (00237) 33129846
TEL CG (00242) 057388009
BP 1155 Pointe Noire
Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!