Experts
Dear Experts
Good afternoon ,
Background -
SS 304L -18 mm plate is cladded with MONEL 400 by explosion bonding.(6mm)
Ellipsoidal dished end is to be formed (570mm ID).
PFHT by virtue of operating conditions is not envisaged .
Seeking guidance for :
Pl. Suggest
1)Cold forming or
2) Hot forming
Pl. suggest suitable process/any heat treatment with supporting Code/Book reference
Appreciate if somebody Shares any experience with similar combinations
Thanks
Vishwas - IWE