There are only small formal differences. EN 287-1, was a pure European norm and has been withdrawn, because it was changed to an international standard (ISO).
Further EN 287.1 was harmonized to the old Pressure Equipment Directive (PED), 97/23/EC where ISO 9606-1 is harmonized to the new PED, 2014/68/EU.
|
Kind regards Kristian Lund Jepsen Lead Specialist, Piping, Mechanical & Layout