Dilution calculation for inconel to ds groove weld with GTAW

23 views
Skip to first unread message

Hrushikesh Sangamnerkar

unread,
Aug 1, 2015, 12:00:58 AM8/1/15
to Materials & Welding

Dear all,
I have Inconel 600 to SS 304 joint.
Process is GTAW.
Filler wire ERNiCr-3
joint design is single V.
Dilution consider 25%.

How to calculate final weld composition?

Thank you.

Hrushikesh H Sangamnerkar