i am found in my site 4 inch stainless steel (SS) flange face damage ( serration ) almost 5mm. what the process to rectify that and acceptance criteria. can anybody tell me.


regard

Rameez

Mac Palola

unread,
Apr 26, 2017, 6:19:09 AM4/26/17
to Materials & Welding
Rameez,

Look at ASME B16.5 flange face sections carefully.

Depth of allowable defects, especially axial ones are very small.

Normally you need to weld repair overlay and then re-mill to get the face acceptable.


Regards

Mac

Dinesh Somwanshi

unread,
Apr 26, 2017, 9:27:35 AM4/26/17
to materials-welding
Machining tolerance to added under such cases, refacing to be done.

Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER

AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
00919881344135
Skype = dinesh570_1

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/29d810ac-3b1f-4d6b-aedf-1c3ade9a76ca%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages