DIFFERENCE BETWEEN EN-287 OR EN-9606.

296 views
Skip to first unread message

udaya bhaskar

unread,
Dec 30, 2015, 9:41:31 PM12/30/15
to material...@googlegroups.com
Dear sir,

As per EN Stander we need to do WQT.

kINDLY SUGGEST  WHICH STANDERS TO BE FOLLOW ON THESE TWO-EN-287 OR EN-9606.
kINDLY LET US KNOW THE DIFFERENCE BETWEEN THESE TWO


--
uday

george....@gr.bureauveritas.com

unread,
Dec 31, 2015, 2:36:42 AM12/31/15
to udaya bhaskar
‎Check this link. For an new qualification you have to go with 9606


Sent from my BlackBerry 10 smartphone.
From: udaya bhaskar
Sent: Πέμπτη, 31 Δεκεμβρίου 2015 - 04:41
Subject: [MW:24017] DIFFERENCE BETWEEN EN-287 OR EN-9606.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3ROLaM9-TLnWAkwj4cyFczMKjJGq8hf9M6aBOjY7Sq8MWA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Deepak Das

unread,
Dec 31, 2015, 2:36:44 AM12/31/15
to Materials & Welding
Hi,

We need to follow BS EN 9606-1 which supersedes BS EN 287-1.

In BS EN 9606-1, Clause 9.3 has been introduced regarding revalidation of a welder's qualification.

Regards,
Deepak Das.

Dinesh Gaur

unread,
Dec 31, 2015, 2:37:26 AM12/31/15
to material...@googlegroups.com
Dear Uday

This British Standard is the UK implementation of EN ISO 9606-1:2013. It is identical to ISO 9606-1:2012. It supersedes BS EN 287-1:2011 which is withdrawn.


moksh...@yahoo.co.in

unread,
Dec 31, 2015, 2:37:53 AM12/31/15
to material...@googlegroups.com


Sent from my ASUS


-------- Original Message --------
From:udaya bhaskar
Sent:Wed, 30 Dec 2015 19:19:08 +0530
To:material...@googlegroups.com
Subject:[MW:24017] DIFFERENCE BETWEEN EN-287 OR EN-9606.

--
A Comparison of BS EN 287 Part 1.2011 with BS EN ISO 9606: Part 1 - Job Knowledge 130.pdf

pankaj phuse

unread,
Jan 16, 2016, 10:20:36 PM1/16/16
to Materials & Welding
EN 287 is now obsolete

Refer 9606 for welder qualification