Kindly clarify the problem which is as follows,

I have CS wps gtaw+smaw (gtaw upto 8mm thk.) 
I have to weld 8"seh.40 (8.18mm)CS pipe with full TIG as per client requirement.

Can I use the above WPS without SMAW (only GTAW upto 8 mm.thk) 

Thanks & Regards,


saleem manhappulath

unread,
Sep 1, 2025, 7:08:29 AM (9 days ago) Sep 1
to material...@googlegroups.com
Dear Guru 

  You can prepare new wps with the same PQR for GTAW ( Sigle process WPS)

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2B-5weSNU4NhpPFUdSbYTzpH5c2vmOgaQxKpu2C-yW4Dn%2BnSdQ%40mail.gmail.com.

Mohd Amiruddin

unread,
Sep 1, 2025, 7:08:29 AM (9 days ago) Sep 1
to material...@googlegroups.com
What is your weld deposited thickness for GTAW? Is it can achieve 8.18mm when times 2?

saleem manhappulath

unread,
Sep 1, 2025, 7:08:30 AM (9 days ago) Sep 1
to material...@googlegroups.com
But the thickness should be upto 8 mm 


Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs
On Mon, 1 Sep 2025 at 1:59 PM guru <guru...@gmail.com> wrote:

Shoaib Yousuf

unread,
Sep 1, 2025, 8:15:52 AM (9 days ago) Sep 1
to material...@googlegroups.com
You can use GTAW Process upto 8mm only without revising the WPS.



On Mon, 1 Sep 2025 at 1:59 PM guru <guru...@gmail.com> wrote:

james gerald

unread,
Sep 1, 2025, 11:25:26 PM (8 days ago) Sep 1
to material...@googlegroups.com
Under 2 conditions you can use WPS.

1. GTAW +SMAW PQR qualified for GTAW 4mm (2t).

2. Example Pipe A106Gr.B minimum tolerance as given below in snap shot within limits in SA-530

Inline image


Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



guru

unread,
Sep 2, 2025, 4:36:40 AM (8 days ago) Sep 2
to material...@googlegroups.com
Noted. Thanks for your valuable suggestion.

Thanks and regards

sridhar cn

unread,
Sep 3, 2025, 7:40:01 AM (7 days ago) Sep 3
to material...@googlegroups.com
 If your WPS/PQR states GTAW is qualified up to 8 mm, then the 8.18 mm exceeds the limit. Consult with the 
Client and clarify if they will accept the existing WPS with the required adjustments. Otherwise, create a new
WPS that covers GTAW for the thickness of the pipe you are going to use. You cannot use the existing WPS 
without modifications due to the thickness exceeding the specified limit.

C Sridhar.