Dear Gents

Can we use ASTM A194 Grde-7 nus instead of ASTM A194 Grade-4nuts.
Because ASTM A194 Grade-4 nuts removed by the ASTM committee because globally lack of material availability.

Please advise.
Salim

pgos...@rogers.com

unread,
Aug 10, 2020, 4:41:07 PM8/10/20
to material...@googlegroups.com

It should not be a problem, unless hardness and other mechanical properties are within the  specified design ranges . Please read this following blog for general guidance.

 

Thanks.

P.Goswami.P.Eng, IWE.

Independent  & Consulting Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAH1-07WaQZ6VvLwZmwnf--t%3Dv5iBMmWuAigP1daFbF%2BKdHW%3D4g%40mail.gmail.com.


Virus-free. www.avg.com
A194 Grade 4 vs. Grade 7 Nuts.pdf

Dhanabal Jalachandran

unread,
Aug 10, 2020, 11:57:09 PM8/10/20
to material...@googlegroups.com

Dear,

 

Yes this statement was issued back in 2015 or 2016 edition of ASTM A 194, please refer the latest version under Section 7.2

 

Best Regards

 

DHANABAL JALACHANDRAN

Senior Inspector | Yanbu Steel Company

CSWIP 3.2.2 & BGAS Gr 2

 

Sent from Mail for Windows 10


--

Rajavarman

unread,
Aug 12, 2020, 2:04:45 AM8/12/20
to material...@googlegroups.com

In ASTM A194 – 2017, its Section 7.2 Also deleted.

But Still ASME Sec 2 (SA-194) latest edition have Grade 4.

 

Just for information

 

 