Hi All,

Could you advise type/brand name of welding consumables which use to build up for Non-Magnetic Stabilizer P550.
Material properties link: https://www.sbsaleshouston.com/P550.html


Thanks
Bien ND

Chintan

unread,
Mar 19, 2019, 2:33:36 AM3/19/19
to Materials & Welding
Use ER 316 or ER 2594 for builtup / buffer layer
Max interpass temp 150 deg cel

Use durmat NiFD wire for tugsten carbide hardfacing over p550 ( use er316 as buffer layer)

Ahmed Osman

unread,
Mar 19, 2019, 10:56:51 AM3/19/19
to Materials & Welding
Dear Mr. Bien

try this electrode 

EFeMnCr

Best Regards ,
ENG. Ahmed Othman


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Bien ND

unread,
Mar 20, 2019, 7:23:18 AM3/20/19
to Materials & Welding
Did you run a test coupon?
How is the test result, chemical and mechanical test?

Vào 13:33:36 UTC+7 Thứ Ba, ngày 19 tháng 3 năm 2019, Chintan đã viết:

Chintan Raval

unread,
Mar 21, 2019, 6:28:32 PM3/21/19
to material...@googlegroups.com
Share details of drawing requirement & application to have clarity on electrode selection

--
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/EkeUuiTQaTA/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.

BCK 055

unread,
Mar 21, 2019, 9:11:47 PM3/21/19
to Chintan Raval
We received information and requirement as a tible from Client.


Sent from my Blackberry
From: Chintan Raval
Sent: Friday, March 22, 2019 05:28
Subject: Re: [MW:29329] Re: Build up material Non-Magnetic Stabilizer P550

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages