Tensile specimen size

48 views
Skip to first unread message

sajid ahmad

unread,
Dec 8, 2015, 10:41:52 PM12/8/15
to material...@googlegroups.com
Dear experts
I have raw material which details are given bellow.
 Material :                SA 516 Grade 70 N
Thickness of Plate: 50 mm
 I observed during inspection that there is missing of plate mark No.So we are conducting Tensile test in order to co-relate with ASME Sec II.
what will be the specimen size?

Regards

M.S.Ahmad 

pgoswami

unread,
Dec 8, 2015, 11:23:59 PM12/8/15
to material...@googlegroups.com
Please look through Sec-II, Part -A, SA 370 or ASTM- A-370. All necessary details are provided in this standard
 

 

Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist
Ontario,Canada.
ca.LinkedIn.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

All provided answer are personal opinions or personal judgments only. It's not connected with any employers by any means. 

 


From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of sajid ahmad
Sent: Tuesday, December 08, 2015 11:11 AM
To: material...@googlegroups.com
Subject: [MW:23961] Tensile specimen size

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAKkJLfgTkvdo37zehERpkPi_kSQeffMmaYgHGS%2BwB91UeZ2gw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

anand gupta

unread,
Dec 8, 2015, 11:39:41 PM12/8/15
to material...@googlegroups.com
Size will be 50×250 mm

Sent from Yahoo Mail on Android


From:"sajid ahmad" <sajid...@gmail.com>
Date:Wed, 9 Dec, 2015 at 6:41

Subject:[MW:23961] Tensile specimen size

--

CHINTUKUMAR GANDHI

unread,
Dec 11, 2015, 12:05:49 PM12/11/15
to material...@googlegroups.com
Dear member,

Please refer SA 370 of ASME Sec. IIA.

Thanks & regards,


C. R. GANDHI


From: sajid ahmad <sajid...@gmail.com>
To: material...@googlegroups.com
Sent: Tuesday, December 8, 2015 9:40 PM

Subject: [MW:23961] Tensile specimen size