ASME BPV Sec V // T-224 SYSTEM OF IDENTIFICATION ON RT FILMS
84 views
Skip to first unread message
Raghuram Bathula
unread,
May 14, 2021, 1:32:44 AM5/14/21
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials-Welding
This essentially be a permanent identification on each radiograph, no markings or stickers will be allowed for mandatory identification traceable to the film
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials-Welding
Adding to Raghuram's comments - Any fogging or flasher shall not be used as ID on Radiographs in ASME Jobs.
Thank you,
Regards,
S.SENTHILKUMAR
On Friday, 14 May, 2021, 11:02:44 am IST, Raghuram Bathula <raghura...@gmail.com> wrote:
This essentially be a permanent identification on each radiograph, no markings or stickers will be allowed for mandatory identification traceable to the film