| AISI 8630H | |
![]() |
|
| Category | Steel |
| Class | Alloy steel |
| Type | H-steel |
| Common Names | Nickel-chromium-molybdenum steel |
| Designations | Germany: DIN 1.6545 Italy: UNI 30 NiCrMo 2 KB United States: ASTM A304 , SAE J1268 , UNS H86300 |
HiI am not able to find mechanical properties/other details/equivalent of AISI 86 30H.I was wondering if any of the member could throw some light in this regard. All I know is it is to be used as an end fitting for a riser.Thanks
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.