How to qualify WPS ?

154 views
Skip to first unread message

Souravbohray

unread,
Jan 30, 2019, 9:34:05 PM1/30/19
to Materials & Welding
How to qualify WPS for long seam of shell?
How to qualify WPS for CIR seam of shell

Raghuram Bathula

unread,
Jan 31, 2019, 5:53:18 AM1/31/19
to Materials-Welding
why do u want to qualify separately?

Ramin Kondori

unread,
Feb 2, 2019, 2:17:55 AM2/2/19
to material...@googlegroups.com
It is better to prepare a but-weld test coupon.
Then weld it according to your WPS.
Remember to record all the parameters during welding.
Then send your coupon to lab and specify the standard and required tests (and conditions of tests like impact test temp).
Wait for the results.
When you receive the results if they are all accepted then fill out PQR form and receive all parties signatures as per your ITP.
If your tests have rejected sample, then you have to go for re-tests or prepare a new coupon with modified WPS and repeat all over again.

Good luck
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Thu, Jan 31, 2019 at 6:04 AM Souravbohray <ermechsou...@gmail.com> wrote:
How to qualify WPS for long seam of shell?
How to qualify WPS for CIR seam of shell

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Er Sourav Bohray

unread,
Feb 2, 2019, 5:18:46 AM2/2/19
to material...@googlegroups.com
thanks for reply. if i directly prepare 6g pipe wps than it will work for wpa also because shell is consider pipe.actually i teach ond junior he is not getting my point i told if u do plate 3g wps u ur welder essential parameter diameter nd position not cover.

You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/DqJXv9xevr8/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.

Mohamed Muneeb

unread,
Feb 2, 2019, 5:43:53 AM2/2/19
to materials-welding
As per which welding and construction code you want to qualify?

Er Sourav Bohray

unread,
Feb 3, 2019, 12:40:31 AM2/3/19
to material...@googlegroups.com
sec 9 asme.sir i want to know about one topic i m very weak in that topic - production test coupon,simulation test as per asme sec 8 div 1

munee...@gmail.com

unread,
Feb 6, 2019, 12:08:34 AM2/6/19
to materials-welding
Yes what exactly is your clause?


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
munee...@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 

Souravbohray

unread,
Feb 12, 2019, 9:15:56 PM2/12/19
to Materials & Welding
sir i want to make it easy to those people who are fresher i know just make a wps of 6g position it will be done for all except what welding process we used

steel_microbe

unread,
Mar 2, 2019, 9:20:17 PM3/2/19
to Materials & Welding
QW-211 BASE METAL
The base metals may consist of either plate, pipe, or
other product forms. Qualification in plate also qualifies
for pipe welding and vice versa. The dimensions of the test
coupon shall be sufficient to provide the required test
specimens.

Groove-weld test qualifies for fillet welds for all thickness and diameters.

Kannayeram Gnanapandithan

unread,
Mar 2, 2019, 9:39:23 PM3/2/19
to materials-welding
As per ASME, for PQR, Test on Flat 1G will qualify all position if no impact requirements.  For WPQR, 6G will qualify all position. Let us be clear. In same way product form, for wps no restrictions but for welder it is restricted with limitations. 


--

José Juan Jiménez Alejandro

unread,
Mar 3, 2019, 10:45:52 AM3/3/19
to material...@googlegroups.com
Sin Drive de Google.

El dom., 3 de marzo de 2019 9:27 a. m., José Juan Jiménez Alejandro <jjjim...@gmail.com> escribió:
44634.pdf