Hi..
m & Y values for Rubber with steel insert gasket. If any study materials available share or provide the details.

Thanks & Regards, 

George Dilintas

unread,
Sep 27, 2020, 1:39:26 AM9/27/20
to material...@googlegroups.com
check in Table 2-5.1 in ASME BPVC Section VIII-1

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/209237826.638056.1601043715086%40mail.yahoo.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages