Good Morning,

My name is Zihni Hakim, i'm a college student who's doing an internship
i am doing a research about Ball Valve ASTM A350 LF2 and ASTM A105. I've been told by my mentor to compare between these two,which one is better to be used in pipeline?
Based on the quality and estimated cost, what do you recommend?

Any help would be appreciated
Thank you

-Zihni

anand gupta

unread,
Aug 1, 2016, 2:10:01 AM8/1/16
to material...@googlegroups.com
Dear sir
both are different use.
SA 350 LF 2  for low temp services and
SA 105 FOR HIGHER SERVICES.

THANKS
A P GUPTA



On Mon, 1 Aug, 2016 at 9:14, Zihni Hakim
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/86de3687-b01a-4766-af07-10422f667eac%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

nishant nair

unread,
Aug 1, 2016, 6:13:06 AM8/1/16
to material...@googlegroups.com
It depends upon the kind of service in which the valve is used and more importantly for what purpose its used.

As its rightly mentioned that one is for low tempeature application n another is for high temp.

Regards,
Nishant Nair.


g, 2016 at 9:14 am, Zihni Hakim

Zihni Hakim

unread,
Aug 1, 2016, 10:29:18 PM8/1/16
to Materials & Welding

ohhh i see
Both of these ASTM A350 LF2 and A105 are to be used in pipeline for gas flow with operating pressure about 537 Psig and the design temperature is 130 F, can you tell me which one is better?
and its also hard for me to find the catalog prices for these A350 LF2 and A105, anyone who knows the price? or anyone can tell me how to get to know the price of these ball valves?

Anyway, thank you so much Gupta and Nishant, i really appreciate your help

Best Regard,
zihni