Tolerance for weld bead width

48 views
Skip to first unread message

BALASUBRAMANIAN .GANESAN

unread,
May 21, 2016, 10:43:19 PM5/21/16
to material...@googlegroups.com
Dear Experts,

is there any tolerance for weld bead width in butt joints of shells. 

share your valuable opinions 

--
Regards,

G.Balasubramanian



Kannayeram Gnanapandithan

unread,
May 21, 2016, 11:36:34 PM5/21/16
to materials-welding

Ref iso 5817 or width of bevel plus 10% on either side

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEanu%3D9jeDZ_%3DvPnJtu5WVJ6cawedvomd8vCUYzp9E8qizwprg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.