Welding Machines Calibration

318 views
Skip to first unread message

Tarek Yehia

unread,
Oct 31, 2011, 8:52:19 AM10/31/11
to material...@googlegroups.com
Dear Experts,

can any body tell me what is the recommended procedure for a/m subject and provide me with some written procedure or work instruction but should be based on applicable standard or suitable reference. 

--
Best regards,
 
Tarek Yehia


alireza samimi

unread,
Oct 31, 2011, 11:41:22 AM10/31/11
to material...@googlegroups.com
My dear friend
regarding to your question about calibration of welding machine and another device in welding you can see these standard:
ISO 17662
BS 7570
 
WITH BEST REGARDS

--- On Mon, 10/31/11, Tarek Yehia <t.yeh...@gmail.com> wrote:
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

prem nautiyal

unread,
Oct 31, 2011, 1:40:48 PM10/31/11
to material...@googlegroups.com
Hi Tarek
 
Please refer the following standard: BS 7570 - code of practice for validation of arc welding equipment.
After reading this standard you have to write your own company procedure and include in QA manual.
Visit our group's blog at http://materials-welding.blogspot.com/ wherin this same topic has been discussed in the past.
 
Regards
 
Prem S Nautiyal

Mobile     +91 9004063879 / 9769316004



--- On Mon, 10/31/11, Tarek Yehia <t.yeh...@gmail.com> wrote:


From: Tarek Yehia <t.yeh...@gmail.com>
Subject: [MW:12800] Welding Machines Calibration
To: material...@googlegroups.com

Madhusudan Rout

unread,
Nov 1, 2011, 10:23:24 AM11/1/11
to material...@googlegroups.com
Follow the BS-7570 standard for callibration.
if you need the standard , i can sent you.





Pieper QSI

unread,
Nov 2, 2011, 5:28:45 PM11/2/11
to material...@googlegroups.com

BS 7570 is no longer valid but replaced by EN 50504.

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

Karthik

unread,
Nov 4, 2011, 2:49:47 AM11/4/11
to material...@googlegroups.com
Hi,
Please find the attached file of sample procedure,It might be useful to you
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282
WELD UNIT METER CERTIFICATION PROCEDURE.pdf

rajeev arora

unread,
Nov 4, 2011, 5:46:58 AM11/4/11
to material...@googlegroups.com
Hello Mr. Karthik ,

can you give some data or detail for function test of the welding machine.

Regards

Rajeev
Regards,

Rajeev Arora
0066-854490697
0066-818706419