Dear Exports 
I have piping to fitting welding but always we have to keeping distance between two seam welds 
Somebody said shall be 90 degree to be distance between two seam weld but I;m not sure
So, I would like to ask what is the distance between seam welds for the piping and mention the reference please ?


 Best Regards,

 Eng. Hany Nabil
 Senior QA / QC Welding Engineer
 Egypt Mobile: 002-01225622022


This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

K.S.Unnikrishnan

unread,
Feb 14, 2022, 11:48:24 PM2/14/22
to material...@googlegroups.com
It is depending on size of the pipe, Min 100 MM also acceptable as per shell DEP.

 
Best regards,
 
K.S.Unnikrishnan




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmTgBzKWscEPP_mbPVb2WiiyYGLwD1OOZDjzwBLn4_OFAw%40mail.gmail.com.

pradip kumar Sil

unread,
Feb 16, 2022, 10:22:10 PM2/16/22
to materials-welding
Hi Nabil,

Pls find below an extract from ARAMCO SAES W-011

image.png
 Every client has a different opinion, so go with the client specification.

Regards,

Pradip

udaya bhaskar

unread,
Feb 17, 2022, 10:24:00 PM2/17/22
to material...@googlegroups.com
Mr.Hany,
Check do you've any client specification, if not follow the API1104 and the distance between the weld seams depends on application & technical data(i.e.,Dia of pipe,thk,Mat.grade,pressure ..........)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmTgBzKWscEPP_mbPVb2WiiyYGLwD1OOZDjzwBLn4_OFAw%40mail.gmail.com.


--
With Regards

Udaya bahaskar.D

Unnikrishnan K.S

unread,
Feb 19, 2022, 12:01:52 AM2/19/22
to material...@googlegroups.com
You described about circumferential weld not long seam 

Thanks and Regards,

K.S.Unnikrishnan
Kollara

On 18-Feb-2022, at 7:24 AM, udaya bhaskar <dus...@gmail.com> wrote: