welding electrode selection fro API 5L X70 grade pipe

1,086 views
Skip to first unread message

Chandra Bhanu Mohapatra

unread,
May 9, 2020, 11:31:55 PM5/9/20
to material...@googlegroups.com
Dear Expert
                   Can anybody suggest me the electrode selection for cross country pipeline with  grade of API 5L X70

--
tHanks & rEgards
Chandra Bhanu Mohapatra

Vinay Thattey

unread,
May 16, 2020, 6:24:48 AM5/16/20
to material...@googlegroups.com
E7018

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG21BZ8UiYpX3LSVhJT2Bte13s%2BB2Az%2BPgVq74jy9_gOs%3DDXBw%40mail.gmail.com.

gbr...@gmail.com

unread,
May 17, 2020, 2:07:48 AM5/17/20
to material...@googlegroups.com

Electrode selection will depend some on wall thickness and welding process.

 

If using stick welding (SMAW) you should try to overmatch strength of electrode to actual pipe yield and tensile strength especially for X70 pipe.  X70 pipe actual yield strength is commonly above 85KSI and actual tensile strength above 95KSI.  There are several known pipeline failures where E80XX and E70XX electrodes were used for X70 pipe especially at road crossing tie-in locations where there is more likely external land forces on the pipeline that concentrates high girth welds.  An E9018 or E10018 can be used. Extreme caution is required if an E9010 electrode is used.  It has a tendency to produce weld cracks when wall thickness is greater than 10mm and when sufficient preheat is not used.  One needs to consider the ability of the welders to weld the open root pass and second pass with EXX18 versus EXX10 type electrodes. It is quite common to use EXX10 type electrodes for root pass and second pass and then change to an EXX18 or EXX45 type electrode for fill and cap passes for X70 pipe.

 

There are many good mechanized welding systems and electrodes for X70 if that option is chosen.

 

Work with the pipe mill to get lower end strength for the X70 pipe – max yield 85KSI and max tensile 95KSI is possible.

Khul ke jiyoo kya pata Kaal hoo na hooooooo

unread,
May 17, 2020, 2:07:50 AM5/17/20
to material...@googlegroups.com
I don’t think E7018 is appropriate. If you have established any PQR then kindly share 

Sent from my iPhone

On 16-May-2020, at 3:54 PM, Vinay Thattey <vinay....@gmail.com> wrote:



Chintan

unread,
May 17, 2020, 2:07:50 AM5/17/20
to Materials & Welding
Use E7018 if pwht not required
Use E8018 G if pwht & impact required

Khul ke jiyoo kya pata Kaal hoo na hooooooo

unread,
May 17, 2020, 4:07:35 AM5/17/20
to material...@googlegroups.com
Thanks for the response.
My straight requirement is as follows
Pipe-API 5L x 70 Thickness 17 mm
Welding requirement-Automatic orbital welding
Use-Cross country pipeline
Kindly provide Best suitable welding consumables Or can share any specific PQR
Thanks
Cam


Sent from my iPhone

> On 17-May-2020, at 11:37 AM, Chintan <chin...@gmail.com> wrote:
>
> Use E7018 if pwht not required
> Use E8018 G if pwht & impact required
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ed350fee-d313-4c37-894a-ca3280cf1d8c%40googlegroups.com.

Kannayeram Gnanapandithan

unread,
May 18, 2020, 3:44:37 AM5/18/20
to materials-welding

vinay pawar

unread,
May 20, 2020, 11:32:34 AM5/20/20
to Materials & Welding
Dear Sir

I have established the PQR in our ongoing project in Kuwait with E6010 root and other passes E7018, used this combination for Tie in welds only.
but for mainline we used Automatic mechanized welding process GMAW, production and quality wise the best method to carried out mainline welding.
selection of process and electrode completely depends upon your project spam, size of pipe with respect to thickness.
In India we have done x70 grade pipelines with following electrode
1.E6010-root and 8010 otherpasses,
2.E6010 root, E8010 hot pass and E81T1 Manual FCAW other passes.
3. E6010 root, E9045 P2H4R and FCAW GS other passes.
its all depend on your project client requirements.

With Regards
Vinay Digarse



On Sunday, May 17, 2020 at 11:37:50 AM UTC+5:30, bapun wrote:
I don’t think E7018 is appropriate. If you have established any PQR then kindly share 

Sent from my iPhone

On 16-May-2020, at 3:54 PM, Vinay Thattey <vinay....@gmail.com> wrote:


E7018

On Sun, 10 May 2020 at 09:01, Chandra Bhanu Mohapatra <bapunc...@gmail.com> wrote:
Dear Expert
                   Can anybody suggest me the electrode selection for cross country pipeline with  grade of API 5L X70

--
tHanks & rEgards
Chandra Bhanu Mohapatra

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

Khul ke jiyoo kya pata Kaal hoo na hooooooo

unread,
May 20, 2020, 11:04:43 PM5/20/20
to material...@googlegroups.com
Good information..
Do u have any update regarding automatic orbital welding for same.

Sent from my iPhone

> On 20-May-2020, at 9:02 PM, vinay pawar <vinayp...@gmail.com> wrote:
>
> electrode

Charles Jacob

unread,
May 20, 2020, 11:04:43 PM5/20/20
to material...@googlegroups.com
Dear experts, 

Before using cellulosic electrodes in thermo mechanical processed pipes used in high sulphur environment. Pl consider the effects on sulphur corrosion cracking during operation.

Regards,

Charles V Jacob.


To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1452a4c2-530f-47c0-9f52-df8abdb60056%40googlegroups.com.

Hani Al Masry

unread,
May 20, 2020, 11:04:46 PM5/20/20
to material...@googlegroups.com
You can use E11018 

Regards 
HA


To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1452a4c2-530f-47c0-9f52-df8abdb60056%40googlegroups.com.

vinay pawar

unread,
May 23, 2020, 11:56:01 PM5/23/20
to Materials & Welding
Dear Sir

i have worked with three different welding technique providers for GMAW process.
1. PWT
2 CRC
3 Serimax

this three are the best in market special for pipeline

With Regards
Vinay
9850740287

QA/QC

unread,
Aug 15, 2020, 11:42:24 PM8/15/20
to Materials & Welding
for root E6010 + E9018-G FOR FILL AND CAP