AISI 4145

525 views
Skip to first unread message

mubeen mubeen

unread,
Jul 29, 2011, 1:01:32 PM7/29/11
to material...@googlegroups.com
Hi,

Can anybody help me out in order to weld subject base material with appropriate consumables(Electrode or filler wire), along with its preheat and post weld heat treatment temperatures.

Regards,
Mubeen
QA Engineer

ashish baviskar

unread,
Jul 29, 2011, 2:05:42 PM7/29/11
to material...@googlegroups.com
dear Mubeen,
                        Please tell me which type of welding you are going to use . Whether it is SAW or SMAW or FCAW ? AISI 4145 material are mostly use in API spec 7 , 7-1 products like drill collars, drill pipes , subs etc. and also tell me the application. 


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
ASHISH BAVISKAR
SURVEYOR
ABSIV INDIA PVT LTD.
(ABS Consulting )
CONTACT NO: 9222180936

mubeen mubeen

unread,
Jul 30, 2011, 2:34:49 PM7/30/11
to material...@googlegroups.com
Ashish,

We have in our facility the welding processes like SMAW, SAW, GTAW & GMAW. The reason behind to quality PQR is to weld AISI 4145 Base material for build up and machine back to drawing required dimensions.
Ashish you are right, this material can be used for Tool joints, Drill pipe and Collars manufacturing purposes,because it meets to API minimum Yield strength requirements.


Regards,
Mubeen

Ramin Kondori

unread,
Jul 31, 2011, 8:00:28 PM7/31/11
to material...@googlegroups.com
So it's an overlay job, right...?

Do you need the same mechanical properties as the base metal (4145) or you are overlaying to achieve more hardness or corrosion resistance...?

I mean what are your desired properties for finished weld...?

Ramin  Kondori
   QC/Welding Engineer 
         IWE AT 0070
   

mitesh patel

unread,
Aug 1, 2011, 12:40:15 AM8/1/11
to material...@googlegroups.com
Dear Mubben 

Please Find H/W Attached Doc. Which is help to selection of Welding  consumable ( SMAW & GTAW ) 

Mitesh Patel
Sr, QA/QC Engg


--
electrode selection similar and dissimilar.pdf
Welding Rod Selection 2.pdf
Welding Rod Selection.xls

chris

unread,
Jul 29, 2021, 10:13:53 PM7/29/21
to Materials & Welding
Hello friends;

Was this query answered?
 I am also encountering a similar problem in welding 4145tube to S355.

we are experiencing a lack of fusion on the 4145 tube side.

Preheat given 150°C
Electrodes tried E7018 and E10018
MTC attached. The tube is Quench tempered.

Any suggestions on this?

Thanks in Advance.
Chris
WhatsApp Image 2021-07-29 at 20.05.08.jpeg
Dia 17 Inch Heat 260873 4145.pdf

Simon Krismer

unread,
Nov 29, 2021, 4:26:42 AM11/29/21
to Materials & Welding
150C is way too low for 4145. The HAZ Hardness will be 50-60HRC at that temperature, and you are no doubt getting hydrogen cracking rather than lack of fusion. 
You will need 250C preheat at least, probably higher for the root run. 

Chris Sabu

unread,
Nov 29, 2021, 10:14:22 PM11/29/21
to material...@googlegroups.com
Thanks ;

Infact we cleared this issue 
300 degree was the preheat given .. even we maintained the inter pass temperature above 250 .. finished the welding after 8hrs continuously without any interruptions.. finally gave pwht @ 600 degree with half hr hold .. later slow cooling with the thermal blanket still in place ..
Tempering must have gone away by this process and the tensile also would have come down .. but still we pressure tested it at 300 bar without failure 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fcca7f2f-b10d-4220-84f6-287b8c06ba7en%40googlegroups.com.
--
THANKS AND REGARDS
CHRIS SABU
0559695451