Post weld Heat treatment (S.R) code as per EN std

37 views
Skip to first unread message

udaya bhaskar

unread,
Jul 11, 2016, 4:57:17 AM7/11/16
to material...@googlegroups.com
Dear all,

Post weld Heat treatment (S.R)  code for welds as per 
ASME         : Sec VIII   Dev 1 under table UCS 56

code as per EN Std what ?
--
With Regards

Udyabahaskar.D

Saravanan Sornam

unread,
Jul 12, 2016, 9:05:32 AM7/12/16
to material...@googlegroups.com

Dear Bhaskar,


You can refer the below standard for EN design vessels. 


PD 5500:2015 Specification for unfired fusion welded pressure vessels


Regards,
Saravanan

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RO-e4AadUntT_xsjnweODS9H0km06bhSJSoNeYWYZaw4Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Kannayeram Gnanapandithan

unread,
Jul 12, 2016, 9:05:44 AM7/12/16
to materials-welding
check in ISO13445 or BS EN 12952

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

--