Forging material Cleanliness

294 views
Skip to first unread message

mechse...@gmail.com

unread,
Sep 25, 2015, 3:07:12 AM9/25/15
to Materials & Welding
Dear experts 


Forgings Shall meet a material cleanliness C2/R2/S2 rating , as described in  ASTM E381.


Kindly clarify the above statement . i couldn't find anything in ASTM E381......

Thanks in advance

Selastine 

meisam shokri arfaei

unread,
Sep 28, 2015, 5:50:18 AM9/28/15
to material...@googlegroups.com
Hi

You should review E381 adjuncts.

Regards

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/26d289fd-e0d8-4685-8a0c-fe66b3df999a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer