WPS & PQR Qualification as per UW-13 of ASME Section Viii Division 1 for Corner Joints

24 views
Skip to first unread message

Shivasankar A

unread,
Jun 11, 2026, 4:59:58 AMJun 11
to Materials & Welding
Is it possible to anybody for sharing the WPS & PQR as sample or reference for the Corner Joints as per the ASME Section Viii Division 1 U-13.
if possible kindly share without any company names or hidden it.

Share it to this email Id: shivasa...@gmail.com


Regards,
A.Shivasankar

venkateswara reddy Desireddy

unread,
Jun 11, 2026, 7:17:30 AMJun 11
to material...@googlegroups.com
U 13 don't need special WPS PQR. Butt weld WPS you can use. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/d6d4f99f-4510-43b3-ae3f-905a5c87fc78n%40googlegroups.com.

Bhavani Prasad Emani

unread,
Jun 11, 2026, 7:17:30 AMJun 11
to Materials & Welding
Hi Shivashankar,

I need to clarify important information about your request:

 Important Clarifications:

1. Code Reference Correction

You mentioned ASME Section VIII Division 1 U-13, but the correct reference for Corner Joints is:

ASME Section VIII Division 1, UW-13 (not U-13)

UW-13 covers "Corner Joints for Non-Circular Vessels"

2. ASME Section IX Requirements

For TWP (Welding Procedure Specification) and PQR (Procedure Qualification Record):

These are required by ASME Section IX, NOT Section VIII

Section VIII = Vessel design/construction rules

Section IX = Welding procedure qualification requirements

3. Corner Joint Specifics (UW-13)

According to UW-13:

Corner joints have joint efficiency E = 1.0 (per UW-12 table)

Minimum weld throat requirements must be met

Lab tests required when using Appendix 28 alternative provisions



Thanking you,

With best regards,                                            
           
Bhavani Prasad Emani,
Mob.No: +91 9032585485